Begin at (1800F-2000F) and reduce the heat as I get closer to shape.
Slow heat to 1475F-1525F, soak if necessary and fully quench in pre-heated quench specific oil.
The first cycle is a "snap temper" at 375F for 1 hour. Subsequent tempering is done at temperatures between 400F-500F depending on the desired hardness of the piece.